Author Topic: TMR bonding problem  (Read 1624 times)

0 Members and 1 Guest are viewing this topic.

Aadhityan

  • Guest
TMR bonding problem
« on: January 28, 2017, 18:40 »
Some of the oxides gets bonded with electrode material(Particularly I used nickel with Mgo) after optimization. I tried with different initial length between electrode and the insulator(MgO). Is it normal in TMR? Because in your example section, I found there is no bonding between insulator and the electrode